Refactoriness(SK) |
37 |
|
Porosity(%) |
≤24 |
|
Bulk Density (g/cm²) |
≥2.25 |
|
Cold Crushing Strength(Kg/cm²) |
≥450 |
|
Thermal Shock |
≥20 |
|
Chemical Composition(%) |
Al2O3 |
≥55.0 |
Fe2O3 |
≤2 |